Specifications

Graphene Flake (Non Stacked reduced Graphene Oxide) NSrGO

Flake Size: 5 – 20 microns

Carbon (C): 93-96 %,   Oxygen (O): 3-5 %

Manganese (Mn): 0 – 0.001%, Sulfur (S): ≤ 2%

Surface Area: 500-600 m2/g

Pore Volume: 0.4-0.5 cm3/g

Mean Pore-Size: 2-2.5 nm

Reduced Graphene Oxide SDS

Graphene Oxide Flake

Composition: Carbon (64-65%), Oxygen (32-34%)

Impurity: Manganese (less 0.01%), Sulfur (≤ 3.0 %)

Thickness: 1 atomic layer – at least 90%

Flake size: 0.5 – 5 microns.

Color: Brown

Shape: Powder, Film, Solution (~ 20 g/L)

Solution pH (1 g/L): 2.4 – 2.7

Solution Conductivity (1 g/L): 90 – 60 mS/m

Graphene Oxide SDS

 

GRAPHENE OXIDE SOLUTION

Thickness:  0.8~1.1 nm – at least 98 %.

Flake size: 0.5-5 microns.

Carbon (C): 64-65 %,   Oxygen (O): 34-36 %

Manganese (Mn): 0 – 0.01 %, Sulfur (S): ≤ 3 %

Concentration: 1, 5, & 10 g/L

pH: 1.80, Viscosity: 11.7 cps

 

 Graphene Oxide in Solution SDS